To provide a transparent conductive film laminate which suppresses the generation of curling and outgas.SOLUTION: There is provided a transparent conductive film laminate 100 which comprises a conductive film 10 including a resin film 14 and a conductive membrane 11 and a carrier film 20 which includes a base film 22 containing a polyester-based resin and an adhesive layer 21 arranged on one side of the base film and is temporarily adhered to the conductive film so as to be peelable via the adhesive layer, wherein the carrier film is laminated on a side opposite to the conductive membrane of the conductive film, the base film has a glass transition temperature (Tg) of 150 degrees centigrade or more, the dimensional shrinkage at 145 degrees centigrade is 0.2 percent or less in the first direction and in the second direction orthogonal to the first direction, respectively, and the MIT number is...